In-plane Shear

In-plane Shear

In-plane shear can be produced by performing a tensile or compression test at ± 45° to the fiber direction.

The specimens are cut from plates 
at 45° to the fiber direction. 

DMS or extensometers are used to measure longitudinal and transverse extension. 

The test method is suitable only for extensions of less than 5%. 